Page 102 - 《摩擦学学报》2021年第3期
P. 102
第 3 期 向鹏程, 等: 两种热处理钢轨焊接接头冲击磨损与损伤性能研究 391
heavy-duty lines[J]. Electric Welding Machine, 2018, 48(5): 69–75 hypereutectic rail welded joints produced by two kinds of welding
(in Chinese) [赵曦. 重载线路用新型钢轨闪光焊质量研究[J]. 电焊 processes[J]. Journal of Southwest Jiaotong University, 2021, 56(2):
机, 2018, 48(5): 69–75]. 403–410 (in Chinese) [李炜, 宋伟军, 戴安, 等. 两种焊接工艺下过
[ 5 ] Xu Xiaodi. Time-frequency feature extraction and dynamic 共析钢轨接头的冲击磨损性能[J]. 西南交通大学学报, 2021,
diagnosis method for track short-wave defects[D]. China Academy 56(2): 403–410].
of Railway Sciences, 2019(in Chinese) [徐晓迪. 轨道短波病害时频 [16] Ma Ninshu, Cai Zhipeng, Huang Hui, et al. Investigation of welding
特征提取和动态诊断方法研究[D].北京: 中国铁道科学研究院, residual stress in flash-butt joint of U 71 Mn rail steel by numerical
2019]. simulation and experiment[J]. Materials & Design, 2015, 88:
[ 6 ] Shi Haochuan. The effect of laser surface strengthening on wear and 1296–1309. doi: 10.1016/j.matdes.2015.08.124.
damage properties of rail welding joints[D]. Chengdu: Southwest [17] Desimone H, Beretta S. Mechanisms of mixed mode fatigue crack
Jiaotong University, 2019 (in Chinese) [施浩川. 激光表面强化对钢 propagation at rail butt-welds[J]. International Journal of Fatigue,
轨焊接接头磨损与损伤性能影响[D]. 成都: 西南交通大学, 2019]. 2006, 28(5-6): 635–642. doi: 10.1016/j.ijfatigue.2005.07.044.
[ 7 ] Li Zili, Zhao Xin, Esveld C, et al. An investigation into the causes of [18] Ding Wei, Gao Wenhui, Wang Guishan, et al. Research and
squats —Correlation analysis and numerical modeling[J]. Wear, application of spray quenching on PD3 quenching rail welding
2008, 265(9-10): 1349–1355. doi: 10.1016/j.wear.2008.02.037. Joints[J]. Railway Engineering, 2004, 44(12): 38–39 (in Chinese)
[ 8 ] Song Tian, Xia Bin, Chen Xiaolin. Application and analysis of post- [丁韦, 高文会, 王贵山, 等. PD3淬火钢轨焊接接头线上喷雾淬火
weld heat treatment method for rail[J]. Practical Electronics, 2014, 方 法 的 研 究 与 应 用 [J]. 铁 道 建 筑 , 2004, 44(12): 38–39]. doi:
(3): 206–207 (in Chinese) [宋甜, 夏彬, 陈晓琳. 钢轨焊后热处理方 10.3969/j.issn.1003-1995.2004.12.015.
法 的 应 用 与 分 析 [J]. 电 子 制 作 , 2014, (3): 206–207]. doi: [19] Huang Dan. Study on new rail flash welding process and properties
10.16589/j.cnki.cn11-3571/tn.2014.03.209. of welded joints[D]. Chengdu: Southwest Jiaotong University, 2019
[ 9 ] Li Jinhua. Research on rail welded joint's wear of heavy haul (in Chinese) [黄丹. 新型钢轨闪光焊工艺及焊接接头的性能研究
railway[D]. Beijing: China Academy of Railway Sciences, 2012(in [D]. 成都: 西南交通大学, 2019].
Chinese) [李金华. 重载线钢轨焊接接头磨损研究[D].北京: 中国 [20] Wang Ziru. Research on surface-hardening device and technology of
铁道科学研究院, 2012]. the mobile rail welded joint[J]. Journal of Materials and Metallurgy,
[10] Godefroid L B, Faria G L, Cândido L C, et al. Failure analysis of 2011, 10(2): 142–145 (in Chinese) [王子儒. 移动式钢轨焊接接头
recurrent cases of fatigue fracture in flash butt welded rails[J]. 表面硬化装置及工艺的研究[J]. 材料与冶金学报, 2011, 10(2):
Engineering Failure Analysis, 2015, 58: 407–416. doi: 10.1016/ 142–145]. doi: 10.14186/j.cnki.1671-6620.2011.02.003.
j.engfailanal.2015.05.022. [21] Li Jinhua, Li Li, Ding Wei, et al. Damage analysis of gas pressure
[11] Xie Xuhui, Yu Qingyuan, Li Wei, et al. Wear property of U 71 MnK welding rail joints of heavy haul railway and its prevention
rail weld under rolling contact[J]. Tribology, 2015, 35(3): 315–321 countermeasures[J]. Railway Engineering, 2016, 56(11): 124–128
(in Chinese) [谢旭辉, 于卿源, 李炜, 等. U 71 MnK钢轨焊缝滚动接 (in Chinese) [李金华, 李力, 丁韦, 等. 重载线钢轨气压焊接头伤损
触磨损性能研究[J]. 摩擦学学报, 2015, 35(3): 315–321]. doi: 分 析 与 预 防 对 策 [J]. 铁 道 建 筑 , 2016, 56(11): 124–128]. doi:
10.16078/j.tribology.2015.03.011. 10.3969/j.issn.1003-1995.2016.11.33.
[12] Jiang W J, Liu C, He C G, et al. Investigation on impact wear and [22] Qi Zhengfeng. Principles of metal heat treatment[M]. Beijing:
damage mechanism of railway rail weld joint and rail materials[J]. Machinery Industry Press, 1987: 52-53(in Chinese) [戚正风. 金属热
Wear, 2017, 376-377: 1938–1946. doi: 10.1016/j.wear.2017.02.035. 处理原理[M]. 北京: 机械工业出版社, 1987: 52-53].
[13] Jiang Wenjuan, Xiang Pengcheng, Ding Haohao, et al. Research on [23] Zhang Jianguo, Jing Xionggang. TTT & CCT curve and
rolling wear and damage properties of gas pressure welding joint of microstructure analysis of U 75 V rail after induction heat
U71Mn rail[J]. Tribology, 2020, 40(5): 24–30 (in Chinese) [蒋文娟, treatment[J]. Hot Working Technology, 2010, 39(8): 168–170, 113
向鹏程, 丁昊昊, 等. U71Mn钢轨气压焊焊接接头滚动磨损与损伤 (in Chinese) [张建国, 敬雄刚. U 75 V钢轨TTT曲线、CCT曲线及感
性能研究[J]. 摩擦学学报, 2020, 40(5): 24–30]. doi: 10.16078/ 应热处理的显微组织分析[J]. 热加工工艺, 2010, 39(8): 168–170,
j.tribology.2020014. 113]. doi: 10.14158/j.cnki.1001-3814.2010.08.013.
[14] Wang Yingying, Li Li, Song Hongtu, et al. Study on induction heat [24] Xu Xin.Study on post-welding heat treatment process to refinet the
treatment device and technology of rail mobile flash butt welding[J]. rail base grain size of welded U71Mn rail joints[D]. Beijing: China
Journal of the China Railway Society, 2018, 40(3): 120–125 Academy of Railway Sciences, 2016(in Chinese) [许 鑫 . 细 化
(in Chinese) [王莹莹, 李力, 宋宏图, 等. 钢轨移动闪光焊感应热处 U71Mn钢轨焊接接头轨底晶粒度的焊后热处理工艺研究[D].北
理装置及工艺研究[J]. 铁道学报, 2018, 40(3): 120–125]. doi: 京: 中国铁道科学研究院, 2016].
10.3969/j.issn.1001-8360.2018.03.018. [25] Deng Hanzhong, Meng Xiangfeng. Effects of normalizing on
[15] Li Wei, Song Weijun, Dai An, et al. Impact wear properties of microstructure and mechanical properties of 15MnTi steel welded